Pink fused aluminium oxide contains chromium oxide, which gives the material its pink colour. The incorporation of Cr2O3 into the Al2O3 crystal structure produces a slight increase in hardness and reduced friability compared to brown and white aluminium oxide.

Hardness: 9 mohs
Shape: angular
Density: 3.92 g/cm3